Resolution: standard / high Figure 1.
Typical tensile stress–strain curves. Of pure PGS and PGS composites of 5, 10, or 15 wt.% Bioglass®. Note the mechanical
strength and strain at rupture increased simultaneously with the addition of Bioglass®
filler (Chen et al. [2010a]; Liang et al. [2010]).
Chen et al. Progress in Biomaterials 2012 1:2 doi:10.1186/2194-0517-1-2 |